Mechanical Properties Metric English Comments
Compressive Yield Strength 113 MPa
16400 psi
ASTM D695
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren..