Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 7.50 MPa | 1090 psi | at 2% nominal strain; ISO 604 |
Quadrant EPP Cestidurâ„¢ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |