Polymer Property : Compressive Yield Strength = 1080 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 1080 MPa
156000 psi
(0.2% Offset) Thickness not reported for this value
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Flat, 2 Part Heat Treatment, 1.250 inch (31.8 mm) Thickness
Tensile strength (ultimate and yield), shear strength, compressive strength, reduction of area, and elongation values reported here are typical for Hot Finished Flat, 2 Part Heat Treatment, 1.250 in..