Mechanical Properties Metric English Comments
Compressive Yield Strength 1070 MPa
155000 psi
Materion moldMAX® HH High Hardness Beryllium Copper Alloy
Description: moldMAX® and PROtherm® are Brush Wellman's copper beryllium alloys specifically designed for the plastic processing industry. These alloys provide a combination of thermal con..
Compressive Yield Strength 1070 MPa
155000 psi
0.2%, hardened to 40 HRC
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha..