Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1045 MPa | 151500 psi | (0.2% Offset) |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |