Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 10.8 MPa | 1570 psi | ASTM D695 |
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled
(discontinued **) Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon. |
|||
Compressive Yield Strength | 10.8 MPa | 1560 psi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Yield Strength | 10.8 MPa | 1560 psi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |