Mechanical Properties Metric English Comments
Compressive Yield Strength 1.41 MPa
205 psi
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material
Construction: ±45° XN50. Fiber: Carbon XN50. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be use..
Compressive Yield Strength 1.41 MPa
205 psi
Stabilized
Hexcel® HexWeb® ACG®-1/2 Honeycomb Aluminum Commercial Grade
HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. ..
Compressive Yield Strength 1.41 MPa
205 psi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..