Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1.40 MPa | 203 psi | |
Sawbones Cellular Rigid Polyurethane Foam 7.5 pcf Density Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone .. |
|||
Compressive Yield Strength | 1.40 MPa | 203 psi | at 5% deformation, parallel to thickness |
Zircar Refractory Composites ZIRCAL-18 Refractory Board Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m.. |
|||
Compressive Yield Strength | 1.40 MPa | 203 psi | Stabilised |
Hexcel® HexWeb® CRF-3/8-ACG-.002-2.3 Chromate free ACG® Honeycomb Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app.. |
|||
Compressive Yield Strength | >= 1.40 MPa | >= 203 psi | ASTM C365 |
Parabeam Industrie Paraglass 10 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |