Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.960 MPa | 139 psi | Static, 70% Compression, ASTM D1621 |
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |