Polymer Property : Compressive Yield Strength = 0.140 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.140 MPa

@Strain 25.0 %
20.3 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Evacell EVA 200 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Compressive Yield Strength 0.140 MPa
20.3 psi
Compressive Load Deflection at 5%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2575 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..
Compressive Yield Strength 0.140 MPa
20.3 psi
Compressive Load Deflection at 5%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2525 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..