Polymer Property : Compressive Yield Strength = 0.0970 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0970 MPa
14.1 psi
at 25% deflection; ASTM D1056
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam
Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing..