Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0896 MPa
13.0 psi
At 10% compression
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Compressive Yield Strength 0.0896 MPa
13.0 psi
At 10% compression
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Compressive Yield Strength 0.0896 MPa
13.0 psi
At 10% compression
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Compressive Yield Strength 0.0896 MPa
13.0 psi
At 10% compression
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..