Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 0.0689 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0689 MPa

@Strain 25.0 %
10.0 psi

@Strain 25.0 %
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft
R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b..
Copyright © lookpolymers.com All Rights Reserved