Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.00689 - 0.0345 MPa @Strain 25.0 % |
1.00 - 5.00 psi @Strain 25.0 % |
0.2"/min. strain rate |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade Thickness: 0.080"- 0.375"Color: BlackInformation provided by Rogers Corporation. |