Mechanical Properties Metric English Comments
Graves Tear Strength 123 kN/m
702 pli
ASTM D1004
DSM Somos® 14120 Water-resistant resin for stereolithography, White
DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p..