Mechanical Properties Metric English Comments
Graves Tear Strength 57.0 kN/m

@Thickness 0.762 mm
325 pli

@Thickness 0.0300 in
extruded sheet; ASTM D624
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.