Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 77.0 kN/m @Thickness 0.760 mm |
439 pli @Thickness 0.0299 in |
on extruded sheet; ASTM D624 |
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |