Polymer Property : Graves Tear Strength = 316 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 55.4 kN/m
316 pli
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber  (discontinued **)
A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr..