Graves Tear Strength 31.5 kN/m
180 pli
Die C; ASTM D642-54
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Gum Compound  (discontinued **
Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed..