Graves Tear Strength 29.5 kN/m

@Temperature 23.9 °C
168 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer
DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent soft touch feel a..