Mechanical Properties Metric English Comments
Graves Tear Strength 26.3 kN/m

@Temperature 23.9 °C
150 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 1060 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 26.3 kN/m

@Temperature 23.9 °C
150 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 2060 CL Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 26.3 kN/m

@Temperature 23.9 °C
150 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 2265 UT Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..