Mechanical Properties Metric English Comments
Graves Tear Strength 220 kN/m
1260 pli
Die C; ASTM D642-54
DuPont Performance Polymers Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound &n
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..