Polymer Property : Graves Tear Strength = 0.228 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 0.228 kN/m
1.30 pli
ASTM D1004
DuPont Teijin Films Mylar® OB13AF Polyester Film, 150 Gauge
Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s..