Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 67.8 - 70.8 MPa | 9830 - 10300 psi | ASTM D790M |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |