Polymer Property : Flexural Strength = 93000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 641 MPa
93000 psi
Transverse Rupture
Pacific Sintered Materials FN-251-S Invar Powdered Metal
Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals.
Flexural Strength 641 MPa
93000 psi
Transverse Rupture
PSM Industries Pacific Sintered Metals Invar FN-251-S Powdered Metal
Coefficient of thermal expansion equal to glassInformation Provided by Pacific Sintered Metals, a division of PSM Industries