Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 92.8 - 97.0 MPa | 13500 - 14100 psi | ASTM D790 |
3D Systems Accura® 40 Plastic for SLA® Systems 40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a.. |