Polymer Property : Flexural Strength = 91.23 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 91.23 MPa
13230 psi
ASTM D790
E-Polymers TEKANATE® G7010 General Purpose Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
Flexural Strength 91.23 MPa
13230 psi
ASTM D790
E-Polymers TEKANATE® G7013 General Purpose Easy Molding Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
Flexural Strength 91.23 MPa
13230 psi
ASTM D790
E-Polymers TEKANATE® G7010FR General Purpose Flame Retardant Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
Flexural Strength 91.23 MPa
13230 psi
ASTM D790
E-Polymers TEKANATE® G7013FR General Purpose Easy Molding Flame Retardant Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
Copyright © lookpolymers.com All Rights Reserved