Flexural Strength 6.16 MPa
893 psi
at 5% deflection; ASTM D790
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..