Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 61.4 MPa | 8910 psi | ASTM D790 |
Plaskolite Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |
|||
Flexural Strength | 61.4 MPa | 8910 psi | ASTM D790 |
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |