Polymer Property : Flexural Strength = 8540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 58.9 MPa

@Thickness 3.20 mm
8540 psi

@Thickness 0.126 in
5.1mm/min; ASTM D790
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions...