Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 82.9 MPa | 12000 psi | ISO 178 |
Polyplastics Duranex® H7500 Polybutylene Terephthalate (PBT), Low warpage DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |