Flexural Strength 807 MPa
117000 psi
with 3K Plain Weave AS-2 Carbon Fiber; ASTM D790
Zyvex Performance Materials Arovex™ HT 250 Nano-Engineered Composite Prepreg System
Arovex® HT 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (1..