Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 552 MPa | 80100 psi | ASTM D790 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Flexural Strength | 552 MPa | 80100 psi | ASTM D790 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |