Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 80.39 MPa | 11660 psi | ASTM D790 |
BCC Products MB 3500 Urethane Fixture Board MB 3500 is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly sha.. |