Flexural Strength 54.9 MPa
7960 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.
Flexural Strength 54.9 MPa
7960 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Strength 54.9 MPa
7960 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.
Flexural Strength 54.9 MPa
7960 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.