Polymer Property : Flexural Strength = 7900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 54.5 MPa
7900 psi
ASTM D790
Techmer ES HiFill® ASA 814 GY
Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
Flexural Strength 54.5 MPa
7900 psi
ASTM D790
Amco Amalloy® B9336 Polymer Alloy
Amco Amalloy B9336 is a clear performance copolymer with exceptional clarity and toughness.Stiff, with good tensile and flexural strength.Information provided by Amco Plastic Materials.
Flexural Strength 54.5 - 57.9 MPa
7900 - 8400 psi
Ceradyne Thermo-Sil® UHS Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..
Flexural Strength 54.5 MPa
7900 psi
ASTM D790
Amco Amalloy® B9941 Polymer Alloy
Amco Amalloy B9941 is a clear performance copolymer with exceptional clarity and toughness.Good flexural and tensile strength.Information provided by Amco Plastic Materials.