Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 53.955 MPa | 7825.5 psi | |
Shinil Chemical SHINSTAT ABS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |