Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 78.48 MPa | 11380 psi | ASTM D790 |
E-Polymers TEKASTER® F100 low-mid viscosity PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Flexural Strength | 78.48 MPa | 11380 psi | ASTM D790 |
E-Polymers TEKASTER® F101F Fast cycle time PBT Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good.. |