Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 78.45 MPa | 11380 psi | ASTM D790 |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |