Mechanical Properties Metric English Comments
Flexural Strength 52.41 MPa
7601 psi
ASTM D790
Lucent Polymers TPP-130 Polypropylene, Homopolymer, 30% Talc Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.