Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | >= 520 MPa | >= 75400 psi | cold bending |
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Flexural Strength | >= 520 MPa | >= 75400 psi | cold bending |
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |
|||
Flexural Strength | >= 520 MPa | >= 75400 psi | cold bending |
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |