Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.01 MPa | 10880 psi | ASTM D790 |
Aclo Accucomp ABS ABS827L Electroplating Grade |
|||
Flexural Strength | 75.01 MPa | 10880 psi | ASTM D790 |
Aclo Accutech ABS ABS831G10L Glass Reinforced |