Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 73.575 MPa | 10671 psi | |
Shinil Chemical SHINCON PETG Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Flexural Strength | 73.575 MPa | 10671 psi | |
Shinil Chemical SHINFLAME PA-6 GF Flame Retardant Polymer Parts SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |