Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 47.59 MPa | 6902 psi | ASTM D790 |
Lucent Polymers TPP-220 Polypropylene, 20% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |