Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 469 MPa | 68000 psi | |
CeramTec 977 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 977 is a zirconia toughened alumina ceramic designed for use in ballistic protection and ceramic armor. |