Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.8 MPa | 9550 psi | ASTM D790 |
Entec Hyrene® PSCRY 14 General Purpose Polystyrene Available in North America Features: General PurposeRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Strength | 65.8 MPa | 9540 psi | ASTM D-790 |
CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures RenShape 472 is a polyurethane-based board designed for CNC machining of production grade checking and assembly fixtures. It may also be used in prototype thermoforming and vacuum forming tooling a.. |
|||
Flexural Strength | 65.8 MPa | 9550 psi | ASTM-D790 |
Abatron Epotron 5 Clear Liquid Epoxy Adhesive for Structural Bonding Epotron 5 is a clear liquid epoxy adhesive for structural bonding. It is recommended for high-strength, permanent bonding of metal, ceramic, glass, laminates, and most rigid materials. Features: Hi.. |