Mechanical Properties Metric English Comments
Flexural Strength 40.0 - 65.0 MPa
5800 - 9430 psi
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics
For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend..