Polymer Property : Flexural Strength = 6402.7 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 44.145 MPa
6402.7 psi
Shinil Chemical SHINCON PMMA Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..