Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 44.14 MPa | 6402 psi | ASTM D790 |
Lucent Polymers TPP-320 Polypropylene, 20% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |