Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 593 MPa | 86000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Bronze BT-126 Powdered Metal Higher strength structural and bearing bronzeInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Flexural Strength | 593 MPa | 86000 psi | Transverse Rupture |
Pacific Sintered Materials BT-126 Bronze Powdered Metal Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals. |